Sign In | Join Free | My rc363.com |
|
Brand Name : Rongsheng Xinwei
Model Number : JM23 JM26 JM28 JM30 JM32
Certification : ISO9001
Place of Origin : Zhengzhou ,China
MOQ : 25 TONS
Price : 200-800USD
Payment Terms : TT; L/C
Supply Ability : 2000tons /month
Delivery Time : 20-30DAYS
Packaging Details : packed on wooden pallets, with water-proof cover, and tightened with plastic/steel bandages
Application : Industrial Furnace
Color : White
Compressive Strength : 2.0-3.0Mpa
Density : 0.9-1.2g/cm3
Fireproof Performance : Excellent
Flexural Strength : 0.2-0.3Mpa
Heat Preservation : Excellent
Material : Ceramic
Moisture Absorption : ≤1.0%
Shape : Brick
Size : Customized
Thermal Conductivity : 0.05-0.2W/m.K
Thermal Shock Resistance : Good
Thickness : 30-200mm
Rongsheng JM23 JM26 JM28 JM30 JM32 Light Weight Mullite Insulation Firebrick
Description of High Performance Mullite Insulation Brick
Mullite Insulation Brick is a kind of quality refractory insulation materials for resisting high temperature with features of light weight, low thermal conductivity, thermal insulation and high compression strength in the high temperature furnaces or kilns. Mullite Insulation Bricks are mainly used for the top of hot blast stove, stack and bottom of blast furnace, regenerative chamber of glass melting furnace, lining of ceramic high temperature furnace and so on.
Technical Parameter of Mullite Insulation Brick:
Item | Index | ||||
JM23 | JM25 | JM26 | JM27 | ||
Al2O3 % | ≥40 | ≥50 | ≥55 | ≥60 | |
Fe2O3 % | ≤1.0 | ≤1.0 | ≤0.9 | ≤0.8 | |
Apparent porosity % | ≤0.55 | ≤0.80 | ≤0.85 | ≤0.9 | |
Cold Crush Strength MPa | ≥1.0 | ≥1.5 | ≥2.0 | ≥2.5 | |
Permanent Linear Change Rate % | 1230℃×12h | 1350℃×12h | 1400℃×12h | 1450℃×12h | |
-1.5~0.5 | |||||
Thermal Conductivity
W/(m·K) |
200±25℃ | ≤0.18 | ≤0.26 | ≤0.28 | ≤0.32 |
350±25℃ | ≤0.20 | ≤0.28 | ≤0.30 | ≤0.32 | |
600±25℃ | ≤0.22 | ≤0.30 | ≤0.33 | ≤0.36 | |
0.05MPa Refractoriness Under LoadT0.5 ℃ | ≥1080 | ≥1200 | ≥1250 | ≥1300 |
Item | Index | |||
JM28 | JM30 | JM32 | ||
Al2O3 % | ≥65 | ≥70 | ≥77 | |
Fe2O3 % | ≤0.7 | ≤0.6 | ≤0.5 | |
Apparent porosity % | ≤0.95 | ≤1.05 | ≤1.35 | |
Cold Crush Strength MPa | ≥2.5 | ≥3.0 | ≥3.5 | |
Permanent Linear Change Rate % | 1510℃×12h | 1620℃×12h | 1730℃×12h | |
-1.5~0.5 | ||||
Thermal Conductivity W/(m·K) | 200±25℃ | ≤0.35 | ≤0.42 | ≤0.56 |
350±25℃ | ≤0.37 | ≤0.44 | ≤0.60 | |
600±25℃ | ≤0.39 | ≤0.46 | ≤0.64 | |
0.05MPa Refractoriness Under Load T0.5 ℃ | ≥1360 | ≥1470 | ≥1570 |
![]() |
JM23 JM26 Mullite Bricks JM28 JM30 JM32 Light Weight Mullite Insulating Fire Brick Images |