Brand Name : Rongsheng Xinwei
Model Number : JM23, JM26, JM26, JM27, JM28, JM30, JM32
Certification : ISO Certification
Place of Origin : Zhengzhou, Henan, China
MOQ : 1 Ton
Price : 200-800 USD
Payment Terms : TT; L/C
Supply Ability : 2000tons /month
Delivery Time : 20-30DAYS
Packaging Details : packed on wooden pallets, with water-proof cover, and tightened with plastic/steel bandages
Color : Red
Compressive Strength : 10MPa
Fire Resistance : Yes
Flexural Strength : 2.5MPa
Heat Preservation : Excellent
Material : Clay
Shape : Brick
Size : Standard
Sound Insulation : Good
Thermal Conductivity : 0.14W/m.K
Thermal Shock Resistance : Yes
Thickness : 50mm
Water Absorption : 10%
Weight : 2.5kg
Rongsheng Factory Supply Mullite Insulation Brick JM23 JM26 JM28 JM30 Insulating Firebrick
Description of Mullite Insulation Brick JM23 JM26 JM28 JM30
Mullite insulating bricks JM-23, JM-26, JM-28,JM-30 are a type of lightweight refractory material used for insulation.They can directly contact flames,have low thermnal conductivity,low thermal melting,low impurity content,and excellent refractoriness. These bricks exhibit properties such as high temperature resistance, good thermal shock stability,and low thermal conductivity.
Feature of Mullite Insulating Brick:
Product specification of JM23 JM26 JM28 JM30 Mullite Insulation Brick
Item | Index | ||||
JM23 | JM25 | JM26 | JM27 | ||
Al2O3 % | ≥40 | ≥50 | ≥55 | ≥60 | |
Fe2O3 % | ≤1.0 | ≤1.0 | ≤0.9 | ≤0.8 | |
Apparent porosity % | ≤0.55 | ≤0.80 | ≤0.85 | ≤0.9 | |
Cold Crush Strength MPa | ≥1.0 | ≥1.5 | ≥2.0 | ≥2.5 | |
Permanent Linear Change Rate % | 1230℃×12h | 1350℃×12h | 1400℃×12h | 1450℃×12h | |
-1.5~0.5 | |||||
Thermal Conductivity W/(m·K) | 200±25℃ | ≤0.18 | ≤0.26 | ≤0.28 | ≤0.32 |
350±25℃ | ≤0.20 | ≤0.28 | ≤0.30 | ≤0.32 | |
600±25℃ | ≤0.22 | ≤0.30 | ≤0.33 | ≤0.36 | |
0.05MPa Refractoriness Under LoadT0.5 ℃ | ≥1080 | ≥1200 | ≥1250 | ≥1300 |
Item | Index | |||
JM28 | JM30 | JM32 | ||
Al2O3 % | ≥65 | ≥70 | ≥77 | |
Fe2O3 % | ≤0.7 | ≤0.6 | ≤0.5 | |
Apparent porosity % | ≤0.95 | ≤1.05 | ≤1.35 | |
Cold Crush Strength MPa | ≥2.5 | ≥3.0 | ≥3.5 | |
Permanent Linear Change Rate % | 1510℃×12h | 1620℃×12h | 1730℃×12h | |
-1.5~0.5 | ||||
Thermal Conductivity W/(m·K) | 200±25℃ | ≤0.35 | ≤0.42 | ≤0.56 |
350±25℃ | ≤0.37 | ≤0.44 | ≤0.60 | |
600±25℃ | ≤0.39 | ≤0.46 | ≤0.64 | |
0.05MPa Refractoriness Under Load T0.5 ℃ | ≥1360 | ≥1470 | ≥1570 |
![]() |
JM23 JM26 Mullite Insulation Brick JM28 JM30 Insulating Firebrick Images |